Synthesis of Nickel Sulfate Powder from Blast Furnace Ferronickel as Alternative Raw Material for Nickel-Based Battery: Effects of Time Stepping in The Precipitate Filtering Process
Main Article Content
Abstract
The demand for nickel for the manufacture of Nickel Manganese Cobalt (NMC)-type batteries is increasing along with the increasing demand for global electric vehicles. Nickel used in the manufacture of NMC batteries is Nickel (II) Sulfate Hexahydrate (NiSO4.6H2O). This study aims to analyze the effect of variations in the time difference of stepped filtering sludge on the precipitated filtrate. In order to synthesize nickel sulfate, this study uses a nickel source from the ferronickel derived from the sintering and smelting process using a Mini Blast Furnace. After the leaching process using a mixture of H2SO4 and H2O2, the precipitation process was carried out using CaCO3 powder to pH 3.01 at a temperature of 90 °C. The precipitation solution was held at 90°C for 24 hours and stepped filtering of the precipitate formed with variations of 2, 4, 6, and 8 hours (The total time is kept the same, i.e., 24 hours). The crystallization results were then washed and dried. Based on X-Ray Fluorescence (XRF), the best results were obtained in stepped filtering variation every 8 hours with 50.23% Ni content and 90.5% Ni separation efficiency.